Products & Services
Research Projects and Other Items for Purchase
![50 - Tracking Chemistry of Minor Elements - DIS Foundry Member Survey](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_50.jpg)
50 - Tracking Chemistry of Minor Elements - DIS Foundry Member Survey
Abstract:
In the fall of 2012, a foundry member asked if we could survey members to see if people...
![49 - Analysis of Pearlitic Ductile Iron with Enhanced Mechanical Properties](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_49.jpg)
49 - Analysis of Pearlitic Ductile Iron with Enhanced Mechanical Properties
Abstract:
The combination of strength and ductility has been difficult to achieve in the...
![48 - Normalizing Heat Treatments to Develop Improved Properties in Heavy Section Iron](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_48.jpg)
48 - Normalizing Heat Treatments to Develop Improved Properties in Heavy Section Iron
Abstract:
The combination of strength and ductility has been difficult to achieve in the...
![47 - Literature Summary - Deteriorated Graphite in Casting Surfaces](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_47.jpg)
47 - Literature Summary - Deteriorated Graphite in Casting Surfaces
Abstract:
DIS Research has shown that a considerable drop in the fatigue life of ductile iron...
![46 - Optimizing Structure-Property Relationships in Ductile Iron](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_46.jpg)
46 - Optimizing Structure-Property Relationships in Ductile Iron
Abstract:
The purpose of this research study was to identify ways to achieve a higher combination...
![45 - Graphite Shape Degradation at the Surface of Chemically Bonded Sand Molds and Cores](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_45.jpg)
45 - Graphite Shape Degradation at the Surface of Chemically Bonded Sand Molds and Cores
Abstract:
Standard specifications of ductile irons are all based on machined test bars either...
![44 - Effect of Surface Defects on Fatigue Properties of Ferritic Ductile Iron](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_44.jpg)
44 - Effect of Surface Defects on Fatigue Properties of Ferritic Ductile Iron
Abstract:
The fatigue strength of ferritic ductile iron, Grade EN-GJS-400-18U-LT, was determined...
![43 - Dimensional Growth of Ductile Iron Castings During Heat Treatment](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_43.jpg)
43 - Dimensional Growth of Ductile Iron Castings During Heat Treatment
Abstract:
The dimensional changes upon heat treatment were studied in three grades of ductile...
![42 - Nodularity in Coupons](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_42.jpg)
42 - Nodularity in Coupons
Abstract:
A correlation between nodularity and ultrasonic velocity was developed for test...
![40 - Survey of Greensand Properties of Member Foundries](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_40.jpg)
40 - Survey of Greensand Properties of Member Foundries
Abstract:
The sand tests were done in one laboratory known to have many years of expertise in...
![39 - Elimination and Neutralization of Boron in Ductile Irons](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_39.jpg)
39 - Elimination and Neutralization of Boron in Ductile Irons
Abstract:
The presence of small amounts of boron in ductile iron is reported to have multiple and...
![37 - Nodularity, Its Measurement, and its Correlation with the Mechanical Properties of Ductile Iron](https://assets.noviams.com/novi-file-uploads/dis/ecommerce/products/research_project_37.jpg)
37 - Nodularity, Its Measurement, and its Correlation with the Mechanical Properties of Ductile Iron
Abstract:
The relationship between nodularity and mechanical properties in the various SAE grades...