Research Projects
24 - Determination of Ductile Iron Nodularity Using Critically-Refracted Longitudinal Ultrasonic Wav
Abstract:
Determination of Ductile Iron Nodularity Using Critically-Refracted Longitudinal...
23 - Determine the Relationship Between Solidification Time and Mechanical Properties of Heavy Secti
Abstract:
Determine the Relationship Between Solidification Time and Mechanical Properties of...
22 - The Effects of Alloying Elements on the Critical Temperatures in Ductile Iron
Abstract:
The influence of carbon, silicon, manganese, nickel, copper, molybdenum, magnesium and...
21 - Use of Sonic Resonance for the Determination of Dynamic Tear Energy in Ductile Iron
Abstract:
The intent of project 21 was to establish the relationship between dynamic tear energy...
20 - Machinability of Ductile Iron Castings
Abstract:
The current study, which analyzes factors affecting machinability of ductile iron...
19 - Simple Fracture Test for Transition Temperature of Ductile Iron (Extension of DIS Project #18)
Abstract:
In the conclusions from Ductile Iron Society Research Project 18 titled "Impact...
18 - Impact Properties of Ductile Iron by Dynamic Tear Testing
Abstract:
The Charpy vee notched test has been widely used to characterize the impact resistance...
17 - Sulfur in Molding Sand Effect on Flake Graphite at the Cast Surface of Ductile Iron Castings
Abstract:
This project investigated the role of sulfur in molding sand on the formation of a...
16 - Characterization of Inclusions in Ductile Iron Castings
Abstract:
Many factors contribute to inclusion formation in cast metals, and this is particularly...
15 - An Investigation of the Effects of Graphite Parameters on the Fracture Toughness of DI
Abstract:
This experimental program was divided into two phases. In Phase I, a systematic set of...
14 - An Investigation of Factors Affecting the Machinability of Ductile Cast Irons
Abstract:
Users of ductile iron castings who have more than one supplier have been aware of wide...
13 - Influence of the Chemical Analysis of Alloys on the Nodule Count of Ductile Iron
Abstract:
Nodule count can be related to the fineness of structure which in turn influences the...