DUCTILE IRON DATA

FOR DESIGN ENGINEERS

AUSTEMPERED DUCTILE IRON

Figure 4.6a Typical ADI yield strength vs. austempering temperature.

Figure 4.6b  Typical ADI elongation vs. austempering temperature.

fig4_6b.JPG (42776 bytes)