ductile iron
   To Promote the production and application of ductile iron castings Issue 3, 2005   

Ultra-Nod Nodularity Tester Developed by Hickman, Williams & Company

Click to Enlarge
  • Ultrasonic velocity nodularity tester developed by:  Hickman, Williams & Company.
  • Uses small coupons for rapid nodularity check.
  • Excellent for process control for Ductile Iron production.
  • Accurate, fast, repeatable.
  • Minimal training required.
  • Rugged construction.  Stainless steel tank, heavy wall steel frame, copper plumbing.
  • Used on foundry floor close to the molten metal processing area.
  • Manual load/unload.
  • Go/No Go system.
  • Customized to fit individual foundry controls.
  • Can be linked with the foundry process control and data collection.
  • No sample cutting, polishing and microscope reading.
  • Sampling cups can be provided.

Sold Exclusively By: 
Hickman, Williams & Company
Equipment Group Division
330 Detroit Ave. Suite D
Monroe, Mi  48162
Phone:  (734) 243-6110 Fax:  (734) 243-6131
www.hicwilco.com
email:  dvanstone@hilwilco.com

Coupon Accept/Reject Screen
Test Tank with Fixture
Velocity vs. Nodularity in DI
Typical Coupons and Mold
Velocity % Nodularity Velocity* % Nodularity
<2199 79 2230 95
2230 80 2237 97
2207 83 2240 98
2210 86 2244 99
2214 89 2246 100
2222 92 >2247 100
Note:  The above table is for reference only.  Each foundry needs to develop its own calibration values for nodularity acceptance. 

*Absolute values for example 0.2203 inches per microseconds.

View 
Ductile Iron Related 
Publications

Located in Strongsville, Ohio, USA
15400 Pearl Road, Suite 234; Strongsville,Ohio  44136
   Billing Address: 2802 Fisher Road, Columbus, Ohio 43204

Phone (440) 665-3686; Fax (440) 878-0070
email:jwood@ductile.org