   To Promote the production and application of ductile iron castings Issue 2, 2004   

 

Research Committee Report on Spectrograph Set Up Standards

During the past two years the DIS Research Subcommittee on Process Control has been running a comparative study on powered metal set up standards (SUS) produced by ARMI (Analytical Reference Materials International). These standards are not certified for true composition, but since they are made from generally homogeneous powders the entire sample can be used. They should be used for drift correction not curve generation. Typical chemistries are shown in the two tables below.

The DIS tested these two standards at 11 different foundry labs and found them to be statistically acceptable for use. We plan to check with DIS foundry members to see if there are other chemistries needed for set up. If you wish further information or if you want to obtain these standards contact ARMI at www.armi.com.

The standards have the following numbers and chemistries:

  215A 216A
Aluminum 0.037 0.06
Boron   0.037
Carbon 3.5 3.0
Cobalt   0.6
Chromium 0.6 1.5
Copper 0.6 0.08
Manganese 1.3 0.3
Molybdenum 0.5 0.004
Niobium   0.3
Nickel 0.9 2.0
Phosphorus 0.3 0.026
Lead   0.005
Sulfur 0.13 0.001
Silicon 2.1 3.0
Tin 0.17 0.04
Titanium 0.07 0.007
Vanadium 0.5 0.03
Tungsten   0.043
Arsenic   0.03
Bismuth   0.004
Magnesium   0.08
Antimony   0.06
Zinc   0.01
Zirconium   0.05

Back to top

View 
Ductile Iron Related 
Publications

Located in Strongsville, Ohio, USA
15400 Pearl Road, Suite 234; Strongsville,Ohio  44136
   Billing Address: 2802 Fisher Road, Columbus, Ohio 43204

Phone (440) 665-3686; Fax (440) 878-0070
email:jwood@ductile.org