ductile iron
   To Promote the production and application of ductile iron castings Issue 3, 2001   

Cover, page 1, page 2, page 3

Neenah Foundry...people, processes, and capabilities uniquely qualified to meet your needs.


Neenah Foundry Assessment Information
  • Located 100 miles Northwest of Milwaukee, Wisconsin
  • Producing Gray (class 30 and 35) and Ductile Iron castings (D4018, D4512, D5506 and D7003)
  • Annual shipping capacity in excell of 150,000 tons
  • Fully facilitized pattern shop
  • Transportation fleet
Melt Capability

Melt:  Three 72" Refractory line water-cooled Hot Blast cupolas with O2 injection (60 ton/hour)

Duplex:  Three 60 ton Vertical Channel furnaces

Pour:  Three 10 ton and One 6 ton Jünker horizontal channel (pressurized) stopper rod furnaces with in-stream inoculation (Note:  pouring systems have dual inoculators)

Core

Two CB-30 horizontal isocure core machines

  • 45" x 40" platen
  • 350 lbs. maximum core weithg

Two 18 liter Peterle vertical isocure core machines

  • 31.5" x 23.8" platen
  • 100 lbx. maximum core weight

Two 12 liter Peterle vertical isocure core machines

  • 27.5" x 23.8" platen
  • 70 lbs. maximum core weight

Two 12 liter Peterle vertical shell core machines

  • 19.6" x 17.9" platen
  • 35 lbs. maximum core weight
Molding

One 2013 Mark 4 Disamatic molding machine

  • Mold size is 21" x 25.6"
  • 100 lbs. maximum pour weight
  • Up to 410 molds/hour

Two 2070 Type B Disamatic molding machines

  • Mold size is 31.5" x 37.4"
  • 275 lbs. maximum pour weight
  • automatic pattern changing system
  • automatic core setting
  • up to 260 molds/hour per machine

One BMD air impulse molding line.

  • 44" x 50" flasks with 10" cope and 16" drag heights
  • 500 lbs. maximum pour weight
Other

Fully facilitized process control labs, paint line, complete casting engineering services.

2121 Brooks Avenue
Box 729
Neenah, WE  54957
Phone:  920 725-7000
Fax:  920 729-3682

 

View 
Ductile Iron Related 
Publications

Located in Strongsville, Ohio, USA
15400 Pearl Road, Suite 234; Strongsville,Ohio  44136
   Billing Address: 2802 Fisher Road, Columbus, Ohio 43204

Phone (440) 665-3686; Fax (440) 878-0070
email:jwood@ductile.org