Foundry Virtual Tour

Dotson Company, Inc. Virtual Tour at October DIS Meeting

Foundry Layout  - Back to Dotson article

Statistics

  • Recycle 8,500 Tons of Steel Per Year
  • 180,000 lbs. Melted Daily
  • 500,000 lbs. Sand Mixed Daily
  • 1,000,000 Molds Per Year
  • 3,000,000 Castings Per Year
  • $100,000 Monthly Energy Costs
  • 120 Employees


   