WELDING, BRAZING, DIFFUSION BONDING, ADHESIVE BONDING

Figure 8.7 Endurance ratios and joint efficiencies for diffusion-bended joints between various grades of Ductile Iron and carbon steel.

fig8_7.GIF (9352 bytes)