DUCTILE IRON DATA

FOR DESIGN ENGINEERS

WELDING, BRAZING, DIFFUSION BONDING, ADHESIVE BONDING

Figure 8.3 Rotating-bending fatigue strength of welded and unwelded pearlitic Ductile Iron.

fig8_3.GIF (5112 bytes)