DUCTILE IRON DATA

FOR DESIGN ENGINEERS

WELDING, BRAZING, DIFFUSION BONDING, ADHESIVE BONDING

Figure 8.1 Relationship between carbon equivalent and no-crack temperature for cast irons.

fig8_1.GIF (9978 bytes)