DUCTILE IRON DATA

FOR DESIGN ENGINEERS

HEAT TREATMENT

Figure 7.12 The effect of tempering temperature on the hardness of oil-quenched Ductile Iron.  The initial hardness was 570 BHN and the tempering time was 2 hours.

fig7_12.GIF (10002 bytes)