DUCTILE IRON DATA
FOR DESIGN ENGINEERS
ALLOY DUCTILE IRONS
Figure 5.8 Effect of temperature on the impact properties of type D-2M Ductile Ni-Resist (1ft-lbf = 1.3558 J).