DUCTILE
IRON DATA
FOR DESIGN ENGINEERS
INTRODUCTION
Figure 2.8 Microstructures and tensile strengths
for various types of Ductile Iron.
| Matrix |
Ferritic
Grade 5 |
Ferritic-
pearlitic
Grade 3 |
Pearlitic
Grade 1 |
Martensitic
(With
retained
austenite) |
Tempered
Martensitic |
ADI
Grade 150 |
ADI
Grade 230 |
Austenitic |
60,000 p.s.i.
(414 mPa) |
80,000 p.s.i.
(552 mPa) |
100,000 p.s.i.
(690 mPa) |
N.A.* |
115,000 p.s.i.
(793 mPa) |
150,000 p.s.i.
(1050 mPa) |
230,000 p.s.i.
(1600 mPa) |
45,000 p.s.i.
(310 mPa) |

|
| *Approximate
ultimate tensile strength 87,000 p.s.i. (600 mPa) Hard, Brittle. (Note that the
magnifications are different.) |
|