DUCTILE IRON DATA

FOR DESIGN ENGINEERS

DESIGNING WITH DUCTILE IRON

Figure 10.2 Methods of correcting shrinkage problems in an isolated heavy section.

fig10_2a.GIF (4167 bytes)
fig10_2b.GIF (2201 bytes)
b)  Add pad for feeding
fig10_2c.GIF (2679 bytes)
c)  Add chills
fig10_2d.GIF (3340 bytes)
d)  Add core to reduce mass